H.H. Shih, L.E. Hornberger, et al.
Journal of Applied Polymer Science
Stress-strain data have been obtained for highly conducting, molecular-macromolecular composites of composition Ni(Pc)I//y/(x)Kevlar, where x and y are respective mole ratios. The modulus of the Ni(Pc)(I//y)/Kevlar materials is affected only slightly at low Ni(Pc)I//y content (Ni(Pc)I//1//. //2/4 . 8 Kevlar equals 5. 8 GPa), but at higher Pc content falls by about 1/3. As the mole fraction of the Ni(Pc)I//y phase increases, elongation-to-break drops, and the fibers become increasingly fragile.
H.H. Shih, L.E. Hornberger, et al.
Journal of Applied Polymer Science
Anagnostis E. Zachariades, Tetsuo Kanamoto
American Institute of Chemical Engineers Annual Meeting 1983
H.H. Shih, L.E. Hornberger, et al.
ACS National Meeting 1984
Anagnostis E. Zachariades, Bin Chung
ANTEC Annual Technical Conference 1985